Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production
Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Grote Afbeelding :  Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

Productdetails:
Plaats van herkomst: China
Merknaam: ZHENAN
Certificering: ISO9001:2015
Modelnummer: FeSiMg 3-8
Betalen & Verzenden Algemene voorwaarden:
Min. bestelaantal: Bespreekbaar
Prijs: Bespreekbaar
Verpakking Details: 1MT grote zak of vanaf klantenverzoek
Levertijd: 7-10 werkdagen na ontvangst van de betaling
Betalingscondities: L/C, T/T, Western Union
Levering vermogen: 2000MT/per maand

Magnesium Ferrosilicon 5% 6% 7% for Spheroidizing Treatment and Nodular Cast Iron Production

beschrijving
Materiaal: Ferro Siliciummagnesium Kleur: Grijs
Chemische samenstelling: Si-Al S P van Fe Vorm: klont
Verpakking: In de Grote Zakken van 1MT Sollicitatie: Staalproductie
Markeren:

Magnesium Ferrosilicon 5% spheroidizing

,

Magnesium Ferrosilicon 6% nodular cast iron

,

Magnesium Ferrosilicon 7% production

Why Spheroidizing Treatment Depends on Magnesium Ferrosilicon 5% 6% 7% Spheroidizing treatment is a controlled reaction, and the alloy is the control. Magnesium ferrosilicon 5% 6% 7% gives the treatment station three settings: a low-magnesium alloy for short, cool pours, a middle alloy for general work, and a high-magnesium alloy for sections that stay liquid long after the ladle is empty. Choose too low and the last metal poured comes out with flake graphite; choose too high